This is a simple flow calibration model for a 0.4mm nozzle.
The walls have a thickness of:
0.8mm
1.2mm
1.6mm
2.0mm
I recommend setting 100% flow first. Layer height 0.2mm.
Then measure the faces of the printout and average.
The average thickness should be 5.6mm ([0.8+1.2+1.6+2.0]/4).
So if you have a different result, substitute that into the formula for x.
y=560/x.
y is your new flow value to set in the slicer.
Repeat the printout with the new settings for verification.
The walls have a thickness of:
0.8mm
1.2mm
1.6mm
2.0mm
I recommend setting 100% flow first. Layer height 0.2mm.
Then measure the faces of the printout and average.
The average thickness should be 5.6mm ([0.8+1.2+1.6+2.0]/4).
So if you have a different result, substitute that into the formula for x.
y=560/x.
y is your new flow value to set in the slicer.
Repeat the printout with the new settings for verification.